  • Silicone common abnormalities and treatment methods

    Silicone common abnormalities and treatment methods

    First, silicone foam common reasons: 1. The mesh is too thin and the printing pulp is thick; Treatment method: Select the appropriate mesh number and reasonable thickness of the plate (100-120 mesh), and bake after appropriately extending the leveling time on the table....
    Read more
  • Knowledge about screen printing silicone ink

    Knowledge about screen printing silicone ink

    1. Basic Knowledge: The ratio of printing silicone ink to Catalyst agent is 100:2. The curing time of Silicone is related to temperature and air humidity. Under normal temperature, when you add curing agent and bake at 120 °c, the drying time is 6-10 seconds. The Operati...
    Read more